Kontakten mit Lieferant

Mr. Liu
Hinterlass eine NachrichtZahlungsart: | L/C,T/T,D/P,Paypal,Money Gram,Western Union |
---|---|
Incoterm: | FOB,CIP |
Minimum der Bestellmenge: | 1 Kilogram |
Lieferzeit: | 30 Tage |
Basisinformation
Modell: Customized
Produktart: Stange
Kohlenstoffgehalt: Mittlerer Kohlenstoff
Product Name: UNS R30605 Stellite 25 Cobalt Alloy L605
Property: Wear And Corrosion Resistance
Material: Cobalt Alloy
Application: Oil&gas Industry
Chemical Composition: Cobalt,chrom,nickel Ect
Color: Silver Grey
HARDNESS: 37-55HRC
Density: 8.15-8.8g/cm
Custom Design: Accept
Size: Customized
Additional Info
Verpakung: Normal export package ,cartons and plywood case
Produktivität: 5000 Kg per month
Marke: XGR
Transport: Ocean,Land,Air
Ort Von Zukunft: Shenyang,Liaoning,China
Versorgungsmaterial-Fähigkeit: 5000 Kg per month
Zertifikate : ISO9001
Hafen: Dalian Port,Qingdao Port,Shanghai Port
Produktbeschreibung
L605 is a cobalt-chromium-tungsten-nickel alloy. L605 displays excellent high-temperature strength and excellent oxidation resistance to 2000°F. The alloy also has good sulfidation resistance and good resistance to wear and galling.
Specifications AMS: 5537, 5759
UNS: R30605
Chemical Composition, %
|
Co |
Cr |
W |
Ni |
Fe |
Mn |
Si |
C |
S |
P |
|
Bal |
20.00 |
15.00 |
10.00 |
3.00 |
1.5 |
.40 |
.10 |
.030 |
.040 |
|
|
|
|
|
MAX |
|
MAX |
|
MAX |
MAX |
Features
Good fabricability
High strength
Resistant to sulfidation, wear and galling
Applications
Good fabricability
High strength
Resistant to sulfidation, wear and galling
Aircraft Engine Components Afterburner Rings
Combustion Liners Turbine Blades
Industrial Furnace Muffles Springs
Valves
Bearings
Mechanical Properties
Temperature |
|||
°F |
°C |
ksi |
MPa |
1200 |
649 |
39 |
270 |
1300 |
704 |
32 |
220 |
1400 |
760 |
24 |
165 |
1500 |
816 |
17 |
120 |
1600 |
871 |
10 |
72 |
1700 |
927 |
6 |
44 |
1800 |
982 |
4 |
25 |
Physical Properties
Density 0.335 lb/in³ 9.27 g/cm³
Melting Range 2426-2570 °F 1300-1410 °C
Specific Heat 0.092 at 70 °F, Btu/lb °F 385 at 21 °C, J/kg °C
Permeability 1.002 at 200 oersted
Thermal conductivity 65 Btuin/ft²h°F 9.4 W/wm°C
Electrical Resistivity 533.2 (75°F) ohm circ mil/ft 0.886 (24°C) microhm-m